2.2.2 焊接结构用轧制钢材
日本焊接结构用轧制钢材 (JIS G 3106—2004) 的性能要求如表2-2-3~表2-2-9所示。
表2-2-3 化学成分
牌号CSiMnPSSM400A厚度≤50mm:≤0.23
厚度>50~200mm:≤0.25-≥2.5×C①≤0.035≤0.035SM400B厚度≤50mm≤:≤0.20
厚度>50~200mm:≤0.22≤0.350.60~1.40≤0.035≤0.035SM400C厚度≤100mm:≤0. 18≤0.35≤1.40≤0.035≤0.035SM490A厚度≤50mm:≤0.20
厚度>50~200mm:≤0. 22≤0.55≤1.60≤0.035≤0.035SM490B厚度≤50mm:≤0.18
厚度>50~200mm:≤0. 20≤0.55≤1.60≤0.035≤0.035SM490C厚度≤100mm:≤0.18≤0.55≤1.60≤0.035≤0.035SM490YA厚度≤100mm: ≤0.20≤0.55≤1.60≤0.035≤0.035SM490YBSM520B厚度≤100mm: ≤0.20≤0.55≤1.60≤0.035≤0.035SM520CSM570厚度≤100mm:≤0.18≤0.55≤1.60 ...... (共2493字) [阅读本文]>>